Trouble with text or images? View this article in your web browser Hello Reader The qualification of welding procedures is one of the most important steps in ensuring weld quality. A welding procedure may look good on paper, but unless it has been tested—or developed within the limits of an accepted prequalified procedure—there is no assurance that it can consistently produce sound welds. As discussed throughout this series, welding quality is not determined by appearance alone. Proper procedure development and qualification are essential for preventing discontinuities such as lack of fusion, cracking, incomplete penetration, and slag inclusions before production welding begins. When fabrication work is governed by codes such as AWS D1.1 Structural Welding Code – Steel or ASME Section IX, those codes specify the exact tests required to qualify a welding procedure. These tests typically involve a combination of destructive and nondestructive examination designed to verify weld integrity and mechanical performance. Even when a code is not required, some form of testing is still advisable whenever a new welding procedure is developed. Why Welding Procedure Qualification MattersThe purpose of qualifying a welding procedure is simple: To verify that the selected welding parameters can produce sound welds. Without qualification testing, fabricators are essentially relying on assumptions. Unfortunately, many shops skip testing entirely when code compliance is not required. This often leads to quality issues that are only discovered after production begins. Procedure qualification testing helps verify:
These tests provide confidence that the welding procedure will perform as intended under real production conditions. 1. Visual Testing (VT)Visual testing is the first inspection step performed during welding procedure qualification. Before destructive testing begins, the weld must first satisfy all applicable visual acceptance criteria. Visual inspection can identify:
Some discontinuities, such as minor porosity, may be acceptable within code limits. Others—particularly cracks—are generally unacceptable in any amount. Although visual inspection is limited to surface conditions, it remains one of the most important quality control tools in welding. 2. Ultrasonic Testing (UT)Ultrasonic testing is a volumetric nondestructive testing method that uses high-frequency sound waves to inspect the weld internally. Unlike visual inspection, UT can detect subsurface discontinuities such as:
Because UT evaluates the entire weld volume, it is widely used in structural and pressure applications where internal weld quality is critical. 3. Radiographic Testing (RT)Radiographic testing, commonly called X-ray inspection, is another volumetric inspection method used during welding procedure qualification. RT works by passing radiation through the weld and recording density differences on film or digital media. Discontinuities such as:
appear as variations in image density. Radiographic testing is especially useful for detecting volumetric discontinuities and is commonly used in pipe welding, pressure vessels, and critical structural applications.
X-ray of an aluminum groove weld showing porosity throughout the weld. 4. Macroetch TestingMacroetch testing is one of the most useful destructive tests for evaluating weld fusion and penetration. A cross-section of the weld is:
This reveals the internal weld profile and allows inspection of:
Macroetches provide immediate visual confirmation of whether the welding procedure is achieving proper penetration and fusion.
A simple macroetch can provide valuable information as to the reliability of a welding procedure. 5. Fillet Break TestMacroetches only show a single cross-section of the weld. Fillet break tests help evaluate fusion over a longer section. In this test:
This allows inspectors to evaluate:
Fillet break tests are commonly used when qualifying fillet weld procedures. 6. Bend TestingBend tests are among the most common destructive tests used in welding procedure qualification. These tests are typically performed on groove welds and are designed to reveal discontinuities that may not be visible externally.
Bend tests will expose discontinuities associated with lack of fusion and slag inclusions. Common bend tests include:
The type of bend test required depends primarily on material thickness and code requirements. Discontinuities such as:
become visible when the specimen is bent. 7. Tension TestingTension testing evaluates the mechanical strength of the weld. A machined specimen is pulled apart using a tensile testing machine to determine:
This test confirms whether the deposited weld metal and welded joint satisfy the required mechanical properties. Tension testing is especially important in structural and pressure-retaining applications where strength is critical. Additional Welding Procedure Qualification TestsThe tests above are some of the most common methods used during welding procedure qualification, but they are not the only options. Additional tests may include:
The required tests depend on:
When Codes Are Not RequiredSome fabrication applications are not governed by structural or pressure vessel codes. In these situations, fabricators may develop:
This is common when code requirements would be unnecessarily restrictive for the application. For example, if welding drip pans or non-structural containment systems, the primary concern may simply be leak prevention rather than mechanical strength. Even in these situations, however, some form of testing should still be performed to verify weld quality. An Alternative: Prequalified Welding ProceduresRather than qualifying procedures through testing, fabricators may also choose to use prequalified welding procedures when permitted by the governing code. Codes such as AWS D1.1 allow prequalification when:
This approach can save significant time and money while still providing reasonable assurance of weld quality. Learning how to write prequalified welding procedures is not compolicated, but a sound understanding and knowing how to follow the governing code is essential. Welding procedure qualification should never be viewed as unnecessary paperwork. Its purpose is to verify that the selected welding process, parameters, and joint design can consistently produce sound welds before production begins. Whether qualification is required by code or developed internally, testing provides valuable information about weld quality and helps prevent costly failures later. References: |
Practical, easy-to-understand welding guidance, real-world examples, and tools to help improve weld quality, productivity, and compliance. For welding professionals including welders, supervisors, inspectors, engineers, and business owners.
Trouble with text or images? View this article on your web browser Hello Reader Galvanized steel is widely used in metal fabrication because of its excellent corrosion resistance. From structural steel components and handrails to trailers, agricultural equipment, and outdoor structures, galvanizing provides a relatively inexpensive way to protect steel from corrosion and extend its service life. However, welding galvanized steel presents challenges that are not encountered when welding...
Trouble with text or images? View this article on your web browser. Hello Reader Competition among welding equipment manufacturers is a great thing. Companies such as Miller, Fronius, OTC, Lincoln Electric, and others continue to develop welding machines that are more capable, easier to use, and increasingly affordable. Welders and manufacturers have benefited tremendously from these advancements. However, there is a potential downside: the belief that better welding equipment is the answer...
Trouble with text or images? View this article on your web browser Hello Reader Few welding discontinuities create more concern than cracks. Unlike porosity, undercut, or excessive reinforcement, cracks are almost never acceptable under structural welding codes because they can significantly reduce the strength and reliability of a welded joint. More importantly, cracks tend to propagate under service loads, meaning a small crack can eventually become a catastrophic failure. Understanding why...